Product Description
*About EKO
FSEKO has been in the field of lamination film for over 10 years. The Lamnition Films are SGS tested with the approval of patent. And the quality is controlled by the quality system ISO 9001: 2008.
*Material
Surface layer: BOPP
Glue layer: EVA adhesive
*Specification
Thickness: 35mic
Width: 300~1800mm
Length: 200~3000m
Paper core: 25.4mm (1 inch), 58mm(2.25inches), 76mm(3 inches)
Bonding: Less than 2



*Process parameter:
Equipment for thermal film: Dry and wet film laminator
Lamination temperature: 95~105c
Roller pressure: 10-20mpa
Speed: 8-20 m/min



*Directions for using BOPP thermal laminating film:
Normal process temperature is 90c-105c, roller pressure and temperature vary with different types of paper, ink and machines.
When using the film for the first time or do other treatment, try a small volume before mass laminating.
Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder.
Make sure put the material in a low-temperature, dry place.
*Packaging:



FSEKO has been in the field of lamination film for over 10 years. The Lamnition Films are SGS tested with the approval of patent. And the quality is controlled by the quality system ISO 9001: 2008.
*Material
Surface layer: BOPP
Glue layer: EVA adhesive
*Specification
Thickness: 35mic
Width: 300~1800mm
Length: 200~3000m
Paper core: 25.4mm (1 inch), 58mm(2.25inches), 76mm(3 inches)
Bonding: Less than 2



*Process parameter:
Equipment for thermal film: Dry and wet film laminator
Lamination temperature: 95~105c
Roller pressure: 10-20mpa
Speed: 8-20 m/min



*Directions for using BOPP thermal laminating film:
Normal process temperature is 90c-105c, roller pressure and temperature vary with different types of paper, ink and machines.
When using the film for the first time or do other treatment, try a small volume before mass laminating.
Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder.
Make sure put the material in a low-temperature, dry place.
SPECIFICATION | 35 micron GLOSS | 35 micronMATT | ||
WEIGHT | m² /kg | 30.63 | 31.65 | |
kg/m² | 0.03265 | 0.0316 | ||
Width | 300 - 1800 mm Upon customer' s requirement | |||
Length | 200 - 3, 000M(more or less 10% allowed) | |||
CoronaTreatment Side | One Side | Both Side | ||
Connector | Less than 2 | |||
Paper Core (inter Diameter) | 25mm(1 inch); 58mm(2.25 inches); 76mm(3 inches) |
*Packaging: