AISI D5 Tool Steel with High Quality (UNS T30405)

Price $5000.00 Compare
Min Order 1 Ton
Shipping From Hunan, China
Popularity 423 people viewed
Quantity
+-
 

Hunan Fushun Metal Co., Ltd.

VIP   Audited Supplier 10 years
Profile Certified by SGS/BV
D5
Alloy Steel Bar
ASTM
Ferrous Steel Scrap
Hot Rolled, Forged
Round, Square, Flat
Grinded, Peeled, Polished, Rough Turned
Mold Steel
Tool Steel Bar
Uns T30405
Diameter: 20-480mm
ASTM-A681
Annealed, Qunched and Tempered
Grinded, Peeled, Polished, Rough Turned
FUSHUN
Apply The Shipping Packing
Diameter: 20-480mm
Hubei, Huangshi
7228600000
Product Description
Similar Grades:
UNS T30405
Shape:
Round, Flat, Square.
Size Range:
 
 Diameter(mm)Thickness (mm)Width (mm)Length(mm)
Round20-480--2000-5800
Square20-480--2000-5800
flat-20-5080-6002000-5800

Steel-making Condition:
EF, EF/EAF+LF+VD, EF/EAF+ESR
Delivery Condition:
Annealed , Quenched + Tempered

Surface Condition:
Black, Grinded, Peeled, Rough turned, Polished

Features:
1.Competitive price
2.Immediate delivery
3.Premium quality
4.Reliable service
5.MOQ: 1 Ton

 
Packing detailsIn seaworthy packing, as your requirement.
Delivery detailswithin 30-50 days
Chemical Composition(%)
 
CMnPSSiCrWVMoCo
1.4-1.600.10-0.60<= 0.030<=0.0300.10-0.6011.00-13.00/1.00max0.70-1.202.50-3.50


Physical Properties
The physical properties of D5 tool steels are outlined in the following table:
 
PropertiesMetricImperial
Density7.7 - 8.03 x 1000 kg/m30.278 - 0.290 lb/in3
Melting point1426°C2600°F


Mechanical Properties
The mechanical properties of D5 tool steels are tabulated below.
 
PropertiesMetricImperial
Poisson's ratio0.27-0.300.27-0.30
Elastic modulus190-210 GPa27557-30457 ksi



Fabrication and Heat Treatment
Heat Treatment
D5 steels should be preheated very slowly up to 815°C (1500°F), then temperature should be increased to 1009°C (1850°F) and held for 20 to 45 minutes. Then they are air quenched.

Forging
Forging of D5 steels can be done at 1065°C (1950°F) down to 1750°F. Do not forge below 926°C (1700°F).

Annealing
Annealing of D5 steels should be done at 886°C (1627°F) followed by slow furnace cooling at 4°C (40°F) per hour or less.

Tempering
D5 steels can be tempered at 204°C (400°F) for achieving Rockwell C hardness of 61 and at 537°C (1000°F) for a Rockwell C hardness of 54.

Applications
Applications of D5 steels include thread rolling, blanking or forming dies operating at temperatures below 482°C (900°F).