250mm 4 Clamps Manual HDPE/PE Pipe Butt Fusion Welding Machine/ Good Service

Price $740.00 Compare
Min Order 1 unit
Shipping From Zhejiang, China
Popularity 490 people viewed
Quantity
+-
 

Zhejiang Huajin Welding Machine Equipment Co., Ltd.

VIP   Audited Supplier 6 years
Profile Certified by SGS/BV
250mm
250mm
Air Cooling
Manual
Intermediate Frequency
AC
Hot Melting
50-60Hz
220V
3kw
131kgs
Huajin
Plywood Cases
250mm
China
8515290000
Product Description

 
ModelHDL250
Pipe size(mm)63mm,75mm,90mm,110mm,125mm,140mm,160mm,180mm,200mm,225mm,250mm
Heating plat Max temp270ºC
Temp deviation in surface(170-250)±5ºC
Max tolerance of welding jointing0.3MM
Working voltage220V
Working frequency50-60HZ
Power/voltage of heating plate2KW / 220V
Power/voltage of planning tool motor1KW / 220V
Total Power3KW
Overall weight of machine(kg)131KGS
Detailed Photos

 
Company Profile

EXHIBITION

OUR MACHINES
Product Parameters
P1: Approach and preheating pressure,
P2: Maximum heating pressure,
P5: Welding pressure,
Pt (Drag pressure): pressure necessary to overcome the friction of the machine. It must be measured by the operator 
with the pressure gauge of the hydraulic unit.

t1, t2, …, t5: duration of phases 1,2, …, 5.

1- Approach and Preheating Phase. Bring the edges to be welded closer with the thermal element at 
the pressure (P1+Pt) so that the edge reaches the dimension provided for by the standard used.

2- Heating Phase. Reduce the pressure to the maximum value P2, sufficient to maintain contact of the edges of the 
pipe with the thermal element, for the time t2

Note: The operator, by reducing the pressure, must be careful not to detach the edges from the thermal element. If 
this happens, the welding must be repeated.

3- Phase of Extraction of the thermal element. Remove the thermal element at the maximum time t3, without damaging the edges of the two elements to be welded.

4- Phase of reaching the welding pressure. Put the edges in contact, progressively increasing the pressure up to the value (P5+Pt), in time t4. Prevent the soft material from coming out of the surfaces that were approached.

5- Welding Phase. Keep the edges in contact under pressure (P5+Pt ) for time t5.

Do not use water or compressed air to accelerate the cooling of the fusion. If necessary, protect the weld from 
rain, wind or excessive solar radiation.

Certifications
FAQ


Q: Are you manufacturer or trading company?
A: We are Manufacturer with more than 10 years foreign trade experience. We have our own factory.
Q: How long is the delivery time ?
A: Depend on the quantity. 

Q: What is your payment term?
A: Sample order :must be 100% in advance by T/T. 
Bulk order :T/T ,30%deposit,70%against copy of B/L. deposit,70%against copy of B/L.

Q: Could i use my own brand ?
A: Yes ,welcome.

Q: Could you provide the after-sale service for the clients after buying your products ?
A: Yes, of course .we supply 24h after-sales service. after delivery, we will track the products for you once every two days,until you get the products. when you got the goods,test them,and give us a feedback. if you have any questions about the problem,contact with us, we will offer the solve way for you.

Q: Do you test all your products before delivery ?
A:Yes,all the products have to pass strict inspection before they go out !

Q: Can you produce base on our drawing &sample ?We may also need our logo on it ?
A :Yes,of course. we do OEM&ODM service. and definitely you can have logo on it.

 

Message Type
* Message Content
* Name  
* Phone
* Email
* CAPTCHA