belongs to the new generation of manually operated splicers, specifically designed for the joining of coarse counts of long staple fibre and continuous filament yarns within a range of Nm 0.1 to 20 Nm(Tex10000-50). Method of application:SKN-2013 type of air splicer can be held in hand or installed on SD-3 aluminum alloy gas supply rail.




Applicable variety of yarn: | yarns used in industries, such as yarn of carpet, BCF, glass fibre, high strength polyester yarn, carbon fibre |
Splicing range: | Nm0.5-Nm12(Tex2000-Tex100) |
Pressure of compressed air: | >0.7Mpa |


1.Product use.
2.Technical parameter and adjustment
2, Yarn count range: 0. 1Nm-20Nm(Tex10000-Tex50)
3, Air pressure: 0.7-0.8Mpa(depends on type of yarn)
4. Adjustment of splicing length: By adjusting the "L" indicator, the yarn overlapping length can be changed. As long as the
strength of joint is satisfied, the shorter the overlapping length, the better for the look of yarn. (the smaller the scale, the
shorter the overlapping length, otherwise longer)
3.The splicing process
The yarn is secured by the yarn clamps, and the scissors cut the surplus yarn. At this stage the chamber cover will close on the mingling chamber.
The ends are retracted towards the mingling chamber. To adjust the length of ends, rotate index "L" .
A jet of compressed air is directed into the mingling chamber and the final joint is made. To adjust the mingling blast rotate index "T" . The chamber cover will now open and the yarn Is ready to be removed. (as shown in tigure 2)

1, Posotion the yarn diagonally, making sure that it is located at the bottom of the introduction slots, this enables the yarn to be crossed in the mingling chamber. | 2, The yarn is secured by the yarn clamps, and the scissors cut the surplus yarn.At this stage the chamber cover will close on the mingling chamber. |

3, The ends are retracted towards the mingling chamber. I o adjust the length ot ends, rotate index "L" | 4, A jet ot compressed air is directer into the mingling chamber and the Tinal Joint is made. o adjust the mingling blast, rotate index "T" .The chamber cover will now open and the yarn is ready to be removed. |
4.Cautions
2, Be careful that the sediment in the mingling chamber may cause block.
3, Make sure the support plate screws, bridge screws and cam plate screws are tightened.
4, Make sure the support screws are not overly tightened, in case the deformation of the support will causes the stiffness
5, Make sure the screws of fastening piece are against the friction disk.
5.Periodical maintenance
Remove the cover pt.390, clean by means of compressed air, and remove fibres and yarns residues by means of tweezers.
2. WEEKLY
Lubricate moving parts with Lubricens (work Jointair while spraying), check the chamber cover movement (correct tunctioning ot springs pt. 152, 156 and 158).
3, EVERY SIX MONTHS
Check the yarn clamps No.216.
Check the cycle speed: if too slow, the Jointair should be overhauled (sludges near the piston or other mechanical obstacles). Provisionally it could be enough to lubricate Jointair inside by spraying Lubriciens near the base inlet nozzle.
LUBRICATION: for the mechanical parts which require grease and pneumatic parts use Kluber Polylub GA 352P.



Contact Us |

We wish you complete success in your business development.
Welcome to visit US.
Air Splicer SKN-2013 splicing for glass fibre and high strength polyester yarn same mesdan
Air Splicer same as mesdan splicing polyester glass fibre wool carbon fibre
Good quality Autoconer air splicer device for autoconer spinning textile machine parts